For melting tests (low melting temperature; +/- 190 ° C).
If the rods are struck with a hammer, the plastic deformation is accompanied by significant heating.
Composition: L-Pb60Sn40 (40% tin)
two sticks: approx.39 cm, approx.550g
Use: 6th grade